Nanomaterials by severe plastic deformation: review of historical developments and recent advances

K Edalati, A Bachmaier, VA Beloshenko… - Materials Research …, 2022 - Taylor & Francis
Severe plastic deformation (SPD) is effective in producing bulk ultrafine-grained and
nanostructured materials with large densities of lattice defects. This field, also known as …

A comprehensive review of magnesium-based alloys and composites processed by cyclic extrusion compression and the related techniques

M Ebrahimi, Q Wang, S Attarilar - Progress in Materials Science, 2023 - Elsevier
Magnesium, its alloys and composites with an approximate density of two-thirds of aluminum
and a quarter of steel are the most prominent engineering materials in various industries …

[HTML][HTML] Corrosion behavior of severely plastically deformed Mg and Mg alloys

A Bahmani, M Lotfpour, M Taghizadeh… - Journal of Magnesium and …, 2022 - Elsevier
Magnesium (Mg) alloys have several advantages, such as low density, high specific strength
and biocompatibility. However, they also suffer weak points, such as high corrosion, low …

State of the art in the photochemical degradation of (micro) plastics: from fundamental principles to catalysts and applications

W Li, W Zhao, H Zhu, ZJ Li, W Wang - Journal of Materials Chemistry A, 2023 - pubs.rsc.org
Plastic, due to its low cost, light weight, and tunable mechanical strength, is one of the most
commonly used materials in daily life. However, the massive production of plastics in the last …

[HTML][HTML] Fine-grained aluminium crossover alloy for high-temperature sheet forming

S Samberger, I Weißensteiner, L Stemper, C Kainz… - Acta Materialia, 2023 - Elsevier
This study presents age-hardenable, fine-grained AlMgZnCu crossover alloys intended for
superplastic and quick plastic forming processes. The study utilizes T-phase (Mg 32 (Al, Zn) …

Combination of severe plastic deformation and heat treatment for enhancing the corrosion resistance of a new Magnesium alloy

PM Kalayeh, M Malekan, A Bahmani, M Lotfpour… - Journal of Alloys and …, 2022 - Elsevier
In the present study, various processes have been carried out on the extruded Mg-4Zn-4Al-
0.6 Ca-0.5 Mn (wt%) alloy to achieve a low corrosion rate Magnesium (Mg) alloy …

Conductive Al alloys: the contradiction between strength and electrical conductivity

Y Wang, L Zhu, G Niu, J Mao - Advanced Engineering Materials, 2021 - Wiley Online Library
In recent years, the severe energy consumption identified in the global power‐transmission
process makes the development of new generation of transmission materials with high …

[HTML][HTML] A study on microstructure development and mechanical properties of pure copper subjected to severe plastic deformation by the ECAP-Conform process

S Atefi, MH Parsa, D Ahmadkhaniha, C Zanella… - Journal of Materials …, 2022 - Elsevier
Commercially pure copper rod was successfully subjected to severe plastic deformation by
applying the continuous equal channel angular pressing (ECAP-Conform) method at room …

An overview on the continuous severe plastic deformation methods

G Faraji, H Torabzadeh - Materials transactions, 2019 - jstage.jst.go.jp
Abstract Severe Plastic Deformation (SPD) processes have been extensively investigated in
the last 30 years to facilitate the production processes of nanostructured (NS) or ultrafine …

Ductility and plasticity of ferritic-pearlitic steel after severe plastic deformation

JA Muñoz, T Khelfa, A Komissarov… - Materials Science and …, 2021 - Elsevier
A ferritic-pearlitic steel was subjected to severe plastic deformation (SPD) through Equal
Channel Angular Pressing (ECAP) at room temperature, obtaining strengths greater than 1 …