[HTML][HTML] High-resolution multiscale modeling of mechanical behavior of cold-drawn pearlitic steels
X Huang, J Wang, S Zhao, Z Yao, C Liu - Journal of Materials Research …, 2021 - Elsevier
A strategy based on representative volume element (RVE) was proposed to investigate the
mechanical behavior of cold-drawn pearlitic steels at multiscale. Firstly, a finite element …
mechanical behavior of cold-drawn pearlitic steels at multiscale. Firstly, a finite element …
Effect of post-weld heat treatment on microstructure, crystallography, and mechanical properties of laser beam welded AISI 904L super austenitic stainless steel
K Ceyhun - Engineering Failure Analysis, 2024 - Elsevier
This research examines the crystallography, microstructure, and mechanical properties of
AISI 904L super austenitic stainless steel (SASS) joint by laser beam welding (LBW). The …
AISI 904L super austenitic stainless steel (SASS) joint by laser beam welding (LBW). The …
[HTML][HTML] Evaluation of microstructural and environmental effects on the hydrogen uptake and desorption in high-strength carbon steels: A thermal desorption …
The hydrogen uptake in three high-strength carbon steels is studied after exposure to three
different environments: an aqueous solution with CO 2 bubbling, CO 2/H 2 S bubbling, and …
different environments: an aqueous solution with CO 2 bubbling, CO 2/H 2 S bubbling, and …
[HTML][HTML] Improvement of tensile properties by controlling the microstructure and crystallographic data in commercial pearlitic carbon-silicon steel via quenching and …
In the current research, a complex microstructure and crystallographic data were developed
through quenching and partitioning (Q&P) process to improve tensile properties of …
through quenching and partitioning (Q&P) process to improve tensile properties of …
[HTML][HTML] Evaluation of the cementite morphology influence on the hydrogen induced crack nucleation and propagation path in carbon steels
The effect of cementite morphology on the crack initiation and growth path was studied using
in situ electrochem-ical micro-cantilever bending (ECCB) technique under hydrogen (H) …
in situ electrochem-ical micro-cantilever bending (ECCB) technique under hydrogen (H) …
Texture and lattice strain evolution in a pearlitic steel during shear deformation: An in situ synchrotron X-ray diffraction study
CSA da Silva, BRC Saraiva, L Novotný… - International Journal of …, 2024 - Elsevier
In-situ synchrotron X-ray diffraction experiments were conducted on the pearlitic steel
sample with a carbon content of 0.74% by weight. Specimens were subjected to uniaxial …
sample with a carbon content of 0.74% by weight. Specimens were subjected to uniaxial …
[HTML][HTML] Assessing the influence of cyclic bending on pearlitic wire's microstructural evolution: a simulation of spiraling and armoring processing effects
PHP Lima, SKB de Lima, MVG Rodrigues… - Journal of Materials …, 2023 - Elsevier
Flexible pipelines are widely used offshore for oil and gas transportation and are subjected
to several complex stress modes during service. Stress tensors cause different alterations in …
to several complex stress modes during service. Stress tensors cause different alterations in …
Effect of Pre-strain on Microstructure, Texture, and Strengthening of Fully Pearlitic Steel
M Masoumi, R de Carvalho Paes Loureiro… - Journal of Materials …, 2022 - Springer
The changes of microstructure, crystallographic texture, and phase/boundary interface in
fully pearlitic industrial steel, under coiling and uncoiling process were comprehensively …
fully pearlitic industrial steel, under coiling and uncoiling process were comprehensively …
Studi Analisis Tahanan Isolasi dan Estimasi Umur Transformator Menggunakan Metode Health Index di PT PLN (Persero) UPT Cawang.
J Sirait, TA Nugroho, S Prayogi - Techno. com, 2024 - search.ebscohost.com
Keandalan operasi transformator sangat tergantung pada kondisi isolasi yang baik.
Penelitian ini bertujuan untuk menganalisis tahanan isolasi dan mengestimasi umur …
Penelitian ini bertujuan untuk menganalisis tahanan isolasi dan mengestimasi umur …
[PDF][PDF] 酸气后冷器封头开裂原因分析
刘民, 鲁美朋, 刘嘉晨, 顾宝兰, 郭静, 孙跃军, 宋明 - 金属热处理 - qikan.cmes.org
某天然气净化厂酸气后冷器浮头式封头内壁出现鼓包和裂纹, 采用宏观检验, 化学成分分析,
硬度测试, 金相检验, 能谱分析, 断口分析及EBSD 测试等方法, 对鼓包和裂纹产生的原因进行了 …