Recent advances in NTC thick film thermistor properties and applications
OS Aleksić, PM Nikolić - Facta universitatis-series: Electronics and …, 2017 - doiserbia.nb.rs
An introduction to thermal sensors and thermistor materials is given in brief. After that novel
electrical components such as thick film thermistors and thermal sensors based on them are …
electrical components such as thick film thermistors and thermal sensors based on them are …
Fabrication and properties of Mn1. 56Co0. 96Ni0. 48O4 free-standing ultrathin chips
Abstract Mn 1.56 Co 0.96 Ni 0.48 O 4 (MCN) free-standing ultrathin chips are successfully
fabricated by using screen printing. The structure, electrical and IR absorption properties …
fabricated by using screen printing. The structure, electrical and IR absorption properties …
Spin Spray‐Deposited Nickel Manganite Thermistor Films For Microbolometer Applications
SW Ko, J Li, NJ Podraza, EC Dickey… - Journal of the …, 2011 - Wiley Online Library
Nickel manganite thin films are good candidates for thermal imaging applications because
of their large temperature coefficient of resistance (TCR),(>− 3%/K) and good environmental …
of their large temperature coefficient of resistance (TCR),(>− 3%/K) and good environmental …
Crystal structure, cation distribution and electrical properties in NixAlyMn3− x− yO4 (0< x< 0.6; 0< y< 0.3) spinel-based NTC chip thermistors
GQ Shao, QJ Cen, ZH Chen, JW Zhang, MX Xie… - Ceramics …, 2024 - Elsevier
Abstract Ni x Al y Mn 3− x− y O 4 (0< x< 0.6; 0< y< 0.3) series NTC chip thermistors with
homogeneous chemical compositions and high-pure spinel phases were fabricated via a …
homogeneous chemical compositions and high-pure spinel phases were fabricated via a …
Far infrared reflectance of sintered Zn2TiO4
MV Nikolić, N Obradović, KM Paraskevopoulos… - Journal of materials …, 2008 - Springer
Zinc-titanate ceramics were obtained by initial mechanical activation in a high-energy
planetary mill for 15 min followed by sintering at temperatures 900–1100° C for 2 h. Room …
planetary mill for 15 min followed by sintering at temperatures 900–1100° C for 2 h. Room …
Infrared optical properties of Mn1.56Co0.96Ni0.48O4 thin films prepared by chemical solution deposition
Abstract∼ 2 μm thick Mn 1.56 Co 0.96 Ni 0.48 O 4 (MCN) films have been prepared on a Al
2 O 3 substrate by the chemical solution deposition method. X-ray diffraction and …
2 O 3 substrate by the chemical solution deposition method. X-ray diffraction and …
Intrinsic resistivity of sintered nickel manganite vs. powder activation time and density
SM Savić, MV Nikolić, OS Aleksić… - Science of …, 2008 - dais.sanu.ac.rs
In this work the DC resistivity of sintered nickel manganite NiMn2O4 (NTC thermistor
material) was studied as a function of additional powder activation time in a planetary ball …
material) was studied as a function of additional powder activation time in a planetary ball …
Micro‐flow sensor for water using NTC thick film segmented thermistors
OS Aleksic, SM Savic, MV Nikolic… - Microelectronics …, 2009 - emerald.com
Purpose–The purpose of this paper is to apply negative thermal coefficient (NTC) thick film
segmented thermistors (TFSTs) in a micro‐flow sensor for water. Design/methodology …
segmented thermistors (TFSTs) in a micro‐flow sensor for water. Design/methodology …
Microstructural and electrical changes in nickel manganite powder induced by mechanical activation
Nickel manganite powder synthesized by calcination of a stoichiometric mixture of
manganese and nickel oxide was additionally mechanically activated in a high energy …
manganese and nickel oxide was additionally mechanically activated in a high energy …
Electrical and transport properties of nickel manganite obtained by Hall effect measurements
Intrinsic resistivity and carrier transport parameters of sintered nickel manganite samples
(NTC thermistor grade) were determined using a Hall effect measurement system based on …
(NTC thermistor grade) were determined using a Hall effect measurement system based on …