Omega phase transformation–morphologies and mechanisms

S Banerjee, R Tewari, GK Dey - International journal of materials …, 2022 - degruyter.com
Various morphologies of the ω phase are observed in the α and the β phases of group-IV
elements and their alloys where formation of this phase is induced by various means …

Microstructure, corrosion behavior and cytotoxicity of Zr–Nb alloys for biomedical application

FY Zhou, BL Wang, KJ Qiu, WJ Lin, L Li… - Materials Science and …, 2012 - Elsevier
In this work, the effects of Nb content on microstructure and corrosion behaviors of
biomedical Zr–Nb alloys were systematically studied. The results of XRD analysis and …

[HTML][HTML] Irradiation damage and hardening in pure Zr and Zr-Nb alloys at 573 K from self-ion irradiation

Q Dong, H Qin, Z Yao, MR Daymond - Materials & Design, 2019 - Elsevier
Zr-ion irradiation was performed on pure Zr, Zr-2.5 Nb, and Zr-5Nb to a dose of 0.5 or 5 dpa
at 573 K. The irradiation induced defects, alloying element redistribution, precipitation, and …

Structurally induced enhancement in corrosion resistance of Zr–2.5% Nb alloy in saline solution by applying ultrasonic impact peening

BN Mordyuk, OP Karasevskaya… - Materials Science and …, 2013 - Elsevier
Near surface layers in Zr–2.5% Nb alloy are modified using severe plastic deformation
process induced by ultrasonic impact peening (UIP). The effect of the UIP processing time …

Terminal solid solubility of hydrogen in Zr-alloy pressure tube materials

RN Singh, S Mukherjee, A Gupta, S Banerjee - Journal of alloys and …, 2005 - Elsevier
In this work, terminal solid solubility (TSS) of hydrogen for Zr-alloy pressure tube materials
was determined corresponding to end of hydride dissolution (TSSD) and start of hydride …

Preparation, structural, microstructural, mechanical and cytotoxic characterization of as-cast Ti-25Ta-Zr alloys

PAB Kuroda, F de Freitas Quadros, KSJ Sousa… - Journal of Materials …, 2020 - Springer
Titanium alloys have been widely used as biomaterials, especially for orthopedic prostheses
and dental implants, but these materials have Young's modulus almost three times greater …

Plastic instability in an omega forming Ti-15% Mo alloy

S Banerjee, UM Naik - Acta materialia, 1996 - Elsevier
The plastic flow behaviour of a β-titanium alloy (Ti-15% Mo) was investigated over a wide
range of temperatures and strain rates covering those conditions where the ω-phase forms …

β-Type Zr–Nb–Ti biomedical materials with high plasticity and low modulus for hard tissue replacements

L Nie, Y Zhan, T Hu, X Chen, C Wang - Journal of the mechanical behavior …, 2014 - Elsevier
In order to develop new biomedical materials for hard tissue replacements, Zr–20Nb–xTi (x=
0, 3, 7, 11 and 15) alloys with required properties were designed and prepared by using the …

Understanding spinodal and binodal phase transformations in U-50Zr

T Yao, A Sen, A Wagner, F Teng, M Bachhav, EIA Anter… - Materialia, 2021 - Elsevier
Engineered spinodal decomposition and spinodal precursors to precipitation hardening are
effective approaches for tailoring material's properties and performance. These approaches …

Irradiation Effects on Stability of δ-UZr2 phase in U-50 wt% Zr Alloy

A Sen, M Bachhav, X Pu, F Teng, T Yao… - Journal of Nuclear …, 2023 - Elsevier
U-50wt% Zr is a candidate metallic nuclear fuel with potential application in light water
reactors due to its excellent thermal properties and high radiation tolerance. The Zr-rich UZr …