[HTML][HTML] A review of additive manufacturing of cermets
Cermets are a category of materials including ceramic and metallic phases, which possess
the combined properties of both phases. Over the last few decades, numerous conventional …
the combined properties of both phases. Over the last few decades, numerous conventional …
A review on the microstructure and properties of TiC and Ti (C, N) based cermets
Cermets are widely used in various industrial applications due to their high hardness,
thermal stability, thermal conductivity, exceptional mechanical properties, and oxidation …
thermal stability, thermal conductivity, exceptional mechanical properties, and oxidation …
[HTML][HTML] Selective laser melting of dispersed TiC particles strengthened 316L stainless steel
Abstract 316L austenitic stainless steel has a wide range of industrial applications. However,
one of the major drawbacks is its low yield strength (170–300 MPa in annealed state). We …
one of the major drawbacks is its low yield strength (170–300 MPa in annealed state). We …
The synergistic effect of grain refinement and precipitation strengthening on mechanical properties and dry sliding wear behavior of medium manganese steels
Z Cai, S Wang, Y Zhou, J Dong, C Yu, L Ma - Tribology International, 2023 - Elsevier
The hot rolled medium manganese Ti-bearing and Ti-free steels were solution treated at
1000℃ and then aged at 500, 550 and 600℃, respectively. The results showed that Ti …
1000℃ and then aged at 500, 550 and 600℃, respectively. The results showed that Ti …
Microstructure evolution and tensile property of high entropy alloy particle reinforced 316 L stainless steel matrix composites fabricated by laser powder bed fusion
X Zhang, D Yang, Y Jia, G Wang… - Journal of Alloys and …, 2023 - Elsevier
Abstract 316 L stainless steel is prone to failure under high-strength conditions due to low
strength and poor wear resistance, which limits its further application severely. In this study …
strength and poor wear resistance, which limits its further application severely. In this study …
Microstructure and nanoindentation behavior of FeCoNiAlTi high-entropy alloy-reinforced 316L stainless steel composite fabricated by selective laser melting
X Zhang, D Yang, Y Jia, G Wang - Materials, 2023 - mdpi.com
Selective laser melting (SLM) is one of the metal additive manufactured technologies with
the highest forming precision, which prepares metal components through melting powders …
the highest forming precision, which prepares metal components through melting powders …
Reaction mechanisms of the TiC/Fe composite fabricated by exothermic dispersion from Fe–Ti–C element system
In this paper, the iron matrix composite TiC/Fe was fabricated by an in-situ process called
exothermic dispersive synthesis from a powder blend of pure elements Fe, Ti and C. The …
exothermic dispersive synthesis from a powder blend of pure elements Fe, Ti and C. The …
Effect of WC addition on TiC reinforced Fe matrix composites produced by laser deposition
H Chen, Y Lu, K Wu, X Wang, D Liu - Surface and Coatings Technology, 2022 - Elsevier
Abstract The TiC/Fe ceramic metal composite (MMC) with WC particles addition was
successfully produced by laser deposition process. The effect of the WC addition to the Fe …
successfully produced by laser deposition process. The effect of the WC addition to the Fe …
[HTML][HTML] Developing the ductility and thermal fatigue cracking property of laser-deposited Stellite 6 coatings by adding titanium and nickel
Y Wu, Y Liu, H Chen, Y Chen, H Li, X Cao - Materials & Design, 2019 - Elsevier
A design strategy is presented for the development of a laser-deposited Stellite 6 coating
with high ductility and low thermal fatigue crack propagation rate. The strategy involved …
with high ductility and low thermal fatigue crack propagation rate. The strategy involved …
In-situ synthesis of TiC/Fe alloy composites with high strength and hardness by reactive sintering
Fe alloy composites reinforced with in-situ titanium carbide (TiC) particles were fabricated by
reactive sintering using different reactant C/Ti ratios of 0.8, 0.9, 1 and 1.1 to investigate the …
reactive sintering using different reactant C/Ti ratios of 0.8, 0.9, 1 and 1.1 to investigate the …