[HTML][HTML] Microstructure evolution, mechanical response and strengthening models for TA15 titanium alloy during thermal processes: A brief review

R Ji, K Zhu, H Zhang, H Luo, J Mao - Journal of Materials Research and …, 2024 - Elsevier
TA15 titanium alloy is widely used in aerospace industry in terms of its high specific strength,
good thermal stability, and excellent corrosion resistance. To further improve its mechanical …

Hot and cold rolling of a novel near-α titanium alloy: mechanical properties and underlying deformation mechanism

Z Jia, Q Zhao, Y Zhang, Y Xu, Y Chen, X Deng… - Materials Science and …, 2023 - Elsevier
In this work, mechanical properties, microstructure evolution mechanism, texture variation
process and deformation mechanism of a near-α CT20 titanium alloy with different hot and …

Fatigue crack growth behavior of an additively manufactured titanium alloy: Effects of spatial and crystallographic orientations of α lamellae

Z Liu, SS Dash, J Zhang, T Lyu, L Lang, D Chen… - International Journal of …, 2024 - Elsevier
Laser-based directed energy deposition (LDED) enables the rapid near-net-shape
fabrication of large-scale titanium components for aerospace applications. However, the …

Deformation behavior and microstructure characteristics of the laser-welded Ti-6Al-4V joint under variable amplitude fatigue

J Chen, H Li, Y Liu, X Zhao, Y Cai, H Chen… - Materials …, 2023 - Elsevier
The deformation behavior and microstructure characteristics of laser-welded Ti-6Al-4V
titanium alloy joints under variable amplitude fatigue ranging from 320 to 380 MPa (initial …

[HTML][HTML] Towards strength-ductility synergy of titanium matrix composites through configuration design: Mesoscale deformation and damage behaviors

X Chen, L Huang, J Song, S Zhou, S Wang… - Composites Part B …, 2024 - Elsevier
A novel multiscale configuration of two-scale network architectures and intragranular
dispersoids was successfully constructed in the (TiBw+ (TiZr) 5 Si 3)/Ti55 composites via …

Plastic slip mechanisms in high-temperature titanium alloys: Insights into silicide and Ti3Al precipitates on ductility

H Zhang, C Zhang, X Liang, R Guo, H Feng, Z Hou… - Scripta Materialia, 2025 - Elsevier
Near-α high-temperature titanium alloys suffer from low ductility due to silicide and α 2 (Ti 3
Al) precipitates. This study explores how adjusting the Al/Zr ratio affects these precipitates …

Tensile deformation behavior of ferrite-bainite dual-phase pipeline steel

X Tu, X Shi, W Yan, C Li, Q Shi, Y Shan… - Materials Science and …, 2022 - Elsevier
In-situ tensile test accompanied by electron backscatter diffraction (EBSD) analyses were
performed on polygonal ferrite (PF) and bainite dual-phase steel, selected regions of interest …

Hierarchical structure and deformation behavior of a novel multicomponent β titanium alloy with ultrahigh strength

X Li, XN Wang, K Liu, GH Cao, MB Li, ZS Zhu… - Journal of Materials …, 2022 - Elsevier
Based on the general [Mo] equivalent criterion and d-electron orbital theory, a new ultrahigh-
strength β titanium alloy with eight major elements (Ti-4.5 Al-6.5 Mo-2Cr-2.6 Nb-2Zr-2Sn-1V …

Achieving an ideal combination of strength and plasticity in additive manufactured Ti–6.5 Al–2Zr–1Mo–1V alloy through the development of tri-modal microstructure

Y Zhang, S Zhang, Z Zou, Y Shi - Materials Science and Engineering: A, 2022 - Elsevier
A better combination of strength and plasticity may be imparted by the tri-modal
microstructure in titanium alloys than the as-built acicular martensite. It is generally …

On the origin of deformation mechanisms in a heterostructured aluminum alloy via slip trace and lattice rotation analyses

SS Dash, DJ Li, XQ Zeng, DY Li, DL Chen - Materials Science and …, 2023 - Elsevier
In this study the micro-deformation mechanisms in an Al–Si cast alloy under stepwise