Effect of chemical degreasing on corrosion stability of components in automobile industry
Š Álló, V Kročko, M Korenko… - Advanced Materials …, 2013 - Trans Tech Publ
This research deals with the corrosion stability of components with a galvanized surface.
The aim is to determine how corrosion resistance is influenced by chemical degreasing. The …
The aim is to determine how corrosion resistance is influenced by chemical degreasing. The …
[HTML][HTML] Detection of corrosion resistance of components in cyclic salt spray
Š Álló, V Kročko, T Ibriksz, J Mareček - … Universitatis Agriculturae et …, 2015 - acta.mendelu.cz
The aim of this research is, to investigate the influence of two types of cyclic salt spray tests
on parts surface treated with galvanizing. On the selected components was performed the …
on parts surface treated with galvanizing. On the selected components was performed the …
[PDF][PDF] The Influence of Thermal Shock on Zn-Ni Surface in the Automobile Industry
Š Álló, V Kročko, P Kangalov, T Ibriksz, M Adamik… - aftmt.uni-ruse.bg
The aim of this research is, to investigate the influence of thermal shock on parts surface
treated with galvanizing. On the chosen components was performed the method Zn-Ni …
treated with galvanizing. On the chosen components was performed the method Zn-Ni …
[PDF][PDF] Controlling and testing methods in the surface treatment
Š Álló, V Kročko, J Žarnovský, M Matúš - conf.uni-ruse.bg
This research contains an investigation of surface treatment and corrosion stability. The
surface treatment was performed on the galvanizing bath-line, it was provided the method …
surface treatment was performed on the galvanizing bath-line, it was provided the method …
Prevádzkové skúšky pôdospracujúcich nástrojov s dvojvrstvou.
R Šoška, P Čičo, R Mikuš - Listy Cukrovarnicke a Reparske, 2014 - search.ebscohost.com
LCaŘ 130, č. 9–10, září–říjen 2014 290 ostria dláta, v ktorej bola vyfrézovaná drážka so
šírkou 20 mm a hĺbkou 2 mm. Vytvorenie tejto drážky zabezpečovalo rovnaký geometrický …
šírkou 20 mm a hĺbkou 2 mm. Vytvorenie tejto drážky zabezpečovalo rovnaký geometrický …
Operational Tests of Double Layered Tillage Tools
R Soska, R Mikus - Listy Cukrovarnické a Reparské, 2014 - search.proquest.com
The results obtained show that the lowest wear resistance was achieved by chisels with no
deposit weld-etalons. Lower wear resistance among the tested hardfacings was reached by …